To fix a stripped thread, coat the fastener with oil, like WD-40 as a release agent, fill the hole with SteelStik, and then place the fastener into the SteelStik-filled hole. As the SteelStik cures, it will form the threading for the bolt. Let SteelStik cure for a few hours, and then unscrew it out.
Full Answer
What color is J-B Weld SteelStik?
J-B Weld Steelstik Set And Cure Color Is Dark Grey Product Features And Strength: J-B Weld Steelstik Has Lap Shear Strength Of 900 Psi, Can Withstand Continuous Temperatures Up To 350F (176C ) And Intermittent Temperatures Of 450F (232C), And Is Chemical Resistant Against Petroleum, Hydraulic Fluids And Other Chemicals When Fully Cured.
Can you use J-B Weld on plastic?
Using J-B Weld on plastic requires that both project pieces are clean and free from grease, oils and residues. This holds true whether repairing a broken plastic component or adhering plastic to another surface, such as fiberglass or metal.
What is the best way to clamp J-B Weld?
Clamp the bonded items or find another way to keep the pieces together as the J-B Weld cures. The best clamping method varies depending on the shapes of the items being bonded. For flat items, a heavy weight may suffice, while in other instances, you may wish to squeeze the items in a vice or hold them together with rubber bands.
What is the difference between SteelStik and Waterweld?
SteelStik is a hand-mixable two part epoxy putty stick that is steel reineforced and non-rusting allowing for quick repairs on anyhing made of metal and more! WaterWeld is a hand mixable two part epoxy putty stick that can cure under water and is ideal fro preparing plumbing, fuel tanks, tubs, showers and more!

How do you use steel stick J-B Weld?
1:043:49How to Use JB Weld SteelStik | Step-by-Step Instructions - YouTubeYouTubeStart of suggested clipEnd of suggested clipIt is the world's strongest bond steel reinforced epoxy jb weld original cold steel and clear weldMoreIt is the world's strongest bond steel reinforced epoxy jb weld original cold steel and clear weld needs to be mixed. So it says cut off a piece i'm not going to use a knife.
How long does it take for J-B Weld steel stick to dry?
SteelStik sets in 3-5 minutes and after 60 minutes, can be drilled, tapped, machined, ground, filed and painted. SteelStik cures to a dark grey color, is rated at a tensile strength of 900 PSI and will withstand temperatures up to 300ºF.
How do you sand a steel stick with J-B Weld?
Start by using a coarse grit to remove the bulk of the JB weld. Then, switch to a finer grit to smooth out the surface. Be careful not to apply too much pressure when sanding the JB weld. This can cause the adhesive to chip or crack.
What will J-B Weld stick to?
J-B Weld can be used to bond surfaces made from metal, porcelain, ceramic, glass, marble, PVC, ABS, concrete, fiberglass, wood, fabric, or paper. Alcohol should be avoided when cleaning surfaces, as it can degrade the bond. J-B Weld is water-resistant, petroleum/chemical-resistant (when hardened), and acid-resistant.
What will J-B Weld not stick to?
Broadly speaking, most J-B Weld products will not adhere or bond well to: Any flexible rubber surface. Canvas. Polypropylene plastic.
How strong is J-B Weld steel?
J-B Weld has a tensile strength of 3960 PSI and sets to a hard bond overnight. It can withstand temperatures up to 550ºF when fully cured.
How long does it take for J-B Weld to set up?
At room temperature, J-B Weld™ sets in 4-6 hours to a dark grey color. A full cure is reached in 15-24 hours. J-B Weld™ has a tensile strength of 5020 PSI and sets to a hard bond overnight. It can withstand temperatures up to 550ºF when fully cured.
How do you prepare metal for J-B Weld?
You'll also want to prep the area to be repaired. For best results, use a detergent or degreaser to first clean the surface. Then roughen it with a file or coarse sandpaper. This will help create a successful and long-lasting bond.
How strong is steel stick?
SteelStik™ sets in 3-5 minutes and after 60 minutes, can be drilled, tapped, machined, ground, filed and painted. SteelStik™ cures to a dark grey color, is rated at a tensile strength of 4000 PSI and will withstand temperatures up to 300ºF.
Is J-B Weld stronger than epoxy?
Weld was accualy better than epoxy. Not price wise, but its quality. JB Weld actually is stronger, but not enough to make it worth it. It's very hard to get smooth.
Which J-B Weld is best for metal?
Original Twin Tube Epoxy J-B Weld is The Original Cold Weld two-part epoxy system that provides strong, lasting repairs to metal and multiple surfaces. Mixed at a ratio of 1:1, it forms a permanent bond with tensile strength of 5020 PSI after curing.
Can you put 2 coats of J-B Weld?
JB Weld can be applied in layers. Just clean the surface thoroughly, apply the JB weld, and wait at least 8 hours to re-apply. When applying additional layers, it's important to wait to apply until the first application is completely cured.
How long does QuikSteel take to set?
CarGo QuikSteel Epoxy Putty with stands up to 500 degrees Fahrenheit temperatures, sets in 5 minutes, is steel hard in 15 minutes and cures in one hour. Cures under water and can be drilled, tapped, filed, sanded and painted.
Can J-B Weld be applied in layers?
Answer: JB Weld can be applied in layers. Just clean the surface thoroughly, apply the JB weld, and wait at least 8 hours to re-apply. When applying additional layers, it's important to wait to apply until the first application is completely cured.
Will J-B Weld work on an exhaust manifold?
JB Weld ExtremeHeat is perfect for making repairs on all manner of high-heat parts, including exhaust manifolds, mufflers, catalytic converters, exhaust pipes, engine blocks, fireplaces, smokers/fireboxes, and many more crack-prone items.
How long does J-B Weld 5 Minute epoxy take to cure?
1 hourJ-B Clearweld is a quick setting, multipurpose two-part epoxy that provides a strong and lasting bond on most surfaces. Clearweld will set in 5 minutes and will fully cure in 1 hour.
How long does it take for JB weld to set?from knowhow.napaonline.com
This particular article is all about KwikWeld, the fast-setting version of JB Weld epoxy. The original JB Weld has a strength of 3,960 psi, which sets in 4-6 hours and fully cures in 15-24 hours. This is great for high-stress items when you have the time to wait, but what if you are sitting on the side of the road because a bracket broke ...
What grit to use for JB welding?from knowhow.napaonline.com
Using JB Weld KwikWeld is just like the original version. Surface preparation is everything. A clean surface is absolutely necessary for a strong, secure repair. Be sure to remove all dirt, grease, oil, or paint from the surface. If you have some cleaner available, like brake cleaner, use that. For smooth surface repairs, we would use a little sandpaper (80 grit is good) to rough up smooth surfaces. If you are dealing with cast iron or aluminum, the rough casting should be good as is once cleaned.
What tool do you use to mix wood?from knowhow.napaonline.com
Use a mixing tool to blend the components together. In the shop, we use a razor blade, but another good item a plastic scraper blade. Cardboard or scrap wood make a perfect mixing board.
Can you mix JB weld with KwikWeld?from knowhow.napaonline.com
If you are dealing with cast iron or aluminum, the rough casting should be good as is once cleaned. Mixing JB Weld KwikWeld is easy, just make sure that you mix both components in equal portions. It does not have to be perfect, but it needs to be pretty close.
What side of the weld do you need to protect?
Also when welding stainless you need to protect the back side of the weld as well as the side you are welding. In fillet welds this is less of an issue but if you are penetrating through the base metal you will get ‘sugaring’ on the back side of the weld.
What does it mean when a weld is hot?
It means that the weld is being exposed to oxygen from the air while it is still hot. This could be caused by :
Why do you need higher pressure for stainless steel?
Higher pressure is generally used to spot weld stainless steel to yield a consistent weld circuit as passivated surfaces of SS require higher pressure to maintain consistent current in the weld junction.
What is the flow rate of a TIG welding?
In TIG welding you generally want to use a fairly large gas lens type ceramic with a gas flow rate of around 8–14 litres per minute.
Why is stainless steel called stainless steel?
The expression stainless comes from one ability to prevent the development of any corrosion product, which may have different color from the base alloy . In cases such as SOME stainless steels, aluminum, titanium alloys, among others, what happen is that some alloying elements react promptly with oxygen atoms and form a stable passive layer, surrounding the base alloy.
How to protect the back of a gas tube?
However ideally the back side needs to be protected. For tube this can be done by back purging ie filling the tube with inert gas. , This is typical done by taping the ends of the tube and running second gas flow inside them (eg with a Y connector and regulator from the gas cylinder). This can generally be achieved with a much lower flow-rate than for the main shielding gas supply.
Can you use flux on the back of a weld?
If back purging isn’t possible you can use an appropriate flux on the back side of the weld but this does mean that the weld will require cleaning afterwards to remove any flux residue.
What is waterweld for PVC?
WaterWeld is yet another plastic-ready product the company offers. It is ideal for PVC pipes or situations in which the plastic parts are wet or will get wet. Clean and rough up the surface of the PVC and then work the two-part epoxy putty together until it reaches a uniform color.
Where to find code for plastic?
These codes are usually found on the bottoms of plastic items, such as containers for food or laundry detergent. Polyethylene is often used for water or gas containers or garden sprayers. Polypropylene is a harder plastic, durable enough for use on some car radiator parts.
How to use JB weld epoxy?
Let the alcohol dry before applying the JB Weld epoxy. Next, use a 1 to 1 ratio of hardener and resin and mix the two until they are the same color. Then, take a scraper and put the epoxy into the crack. You may need to press hard to get the mixture to the back of the crack and really seal it.
What material does JB Weld not work with?
Regular plastic is not the only material JB Weld does not work with. Polypropylene and polyethylene plastics are also not able to bond with this epoxy. Other materials include vinyl, leather, and canvas. If you want to fix a tarp, then you have to use an adhesive designed to work with tarp materials.
Does J-B Weld Work On Aluminum Engine Block?
One of the keys to welding this crack together is that you have to spend a good amount of time making sure the crack is free from paint, rust, and liquids. After cleaning the crack with a wire brush, you should wipe it down with rubbing alcohol.
Can You J-B Weld Aluminum Oil Pan?
As long as the crack is not too large, width-wise, you should have success in using this product on your cracked oil pan. The biggest issue in using this product for that repair is the time it takes to fully cure and be ready for use.
How strong is JB weld?
How Strong is J-B Weld On Aluminum. According to some scientific tests, the tensile strength of JB Weld reaches 5020 psi roughly. To reach that level of strength, you have to allow the epoxy to cure overnight. The set-up time is 4-6 hours and the curing time is between 15 and 24 hours.
What is the best JB weld for aluminum?
Most likely, the best JB Weld product for aluminum would be their Marine Weld option. It is designed for boats that must handle very tough conditions that most RV users do not face. You mix the 2 tubes at a 1 to 1 ratio and after application, you let it sit for 4 to 6 hours and then cure for up to 24.
What kind of sandpaper do you use to sand metal?
Most people are talking about the pre-sanding you have to do before you apply the glue. At that point, you need to use coarse grit sandpaper to rough the metal pieces up.